{"id":20478,"date":"2021-03-23T07:09:01","date_gmt":"2021-03-23T07:09:01","guid":{"rendered":"https:\/\/www.meetyoucarbide.com\/?p=20478"},"modified":"2021-03-23T07:09:48","modified_gmt":"2021-03-23T07:09:48","slug":"efficient-solutions-to-stainless-steel-drilling-issues","status":"publish","type":"post","link":"https:\/\/www.meetyoucarbide.com\/tr\/verimli-cozumler-paslanmaz-celik-delme-sorunlari\/","title":{"rendered":"Paslanmaz \u00c7elik Delme Sorunlar\u0131na Etkili \u00c7\u00f6z\u00fcmler"},"content":{"rendered":"
\n

Paslanmaz \u00e7elik matkap sorunlar\u0131 ile ilgili olarak, esas olarak a\u015fa\u011f\u0131daki d\u00f6rt a\u00e7\u0131dan \u00e7\u00f6z\u00fcl\u00fcr: Do\u011fru ucu se\u00e7in<\/p>\n\n\n\n

Matkap malzemesi uygundur<\/h2>\n\n\n\n

Genellikle W6Mo5Cr4V2Al, w2mo9cr4co8 ve di\u011fer malzemeler kullan\u0131lmal\u0131d\u0131r. Bu malzemelerin dezavantajlar\u0131, pahal\u0131 olmalar\u0131 ve sat\u0131n almalar\u0131n\u0131n zor olmas\u0131d\u0131r. Delme i\u00e7in yayg\u0131n olarak kullan\u0131lan W18Cr4V s\u0131radan standart y\u00fcksek h\u0131z \u00e7eli\u011fi ucunu sat\u0131n al\u0131rken, k\u00fc\u00e7\u00fck tepe a\u00e7\u0131s\u0131n\u0131n eksiklikleri, \u00e7ok geni\u015f tala\u015f\u0131n delikten zaman\u0131nda bo\u015falmas\u0131 nedeniyle, kesme s\u0131v\u0131s\u0131 biti zaman\u0131nda so\u011futamaz ve zay\u0131f termal Paslanmaz \u00e7eli\u011fin iletkenli\u011fi, kesici kenar \u00fczerinde yo\u011funla\u015fan kesme s\u0131cakl\u0131\u011f\u0131 y\u00fckselecek, bu da iki yana ve ana kenar\u0131n yanmas\u0131na ve kenar \u00e7\u00f6kmesine kolayca yol a\u00e7acak ve bitin hizmet \u00f6mr\u00fcn\u00fc k\u0131saltacakt\u0131r D\u00fc\u015f\u00fck.<\/p>\n\n\n\n

\"\"<\/figure>\n\n\n\n

Bit'in geometrik parametreleri makul<\/h2>\n\n\n\n

1. \u00c7apraz kesme kenar\u0131n\u0131n g\u00fcc\u00fcn\u00fc art\u0131rmak i\u00e7in, tepe a\u00e7\u0131s\u0131n\u0131 art\u0131r\u0131n ve ayn\u0131 anda \u00e7apraz kesme kenar\u0131n\u0131 z\u0131mparalay\u0131n.<\/p>\n\n\n\n

Delme i\u00e7in W18Cr4V s\u0131radan y\u00fcksek h\u0131z \u00e7eli\u011fi ucu kullan\u0131ld\u0131\u011f\u0131nda, kesme kuvveti ve kesme s\u0131cakl\u0131\u011f\u0131 matkap noktas\u0131nda yo\u011funla\u015f\u0131r. Bitin kesici k\u0131sm\u0131n\u0131n dayan\u0131kl\u0131l\u0131\u011f\u0131n\u0131 artt\u0131rmak i\u00e7in \u00fcst a\u00e7\u0131 uygun \u015fekilde artt\u0131r\u0131labilir ve \u00fcst a\u00e7\u0131 genellikle 135-140 derecedir.<\/p>\n\n\n\n

The increase of the top angle will also reduce the rake angle of the outer edge and narrow the cuttings, which is conducive to chip removal. However, with the increase of the top angle, the cross edge of the bit becomes wider, which will increase the cutting resistance. Therefore, the cross edge of the bit must be polished. After grinding, the cross edge’s angle is 47-55 degrees, and the front angle of the cross edge is 3-5 degrees. When grinding the transverse edge, the corner between the cutting edge and the cylindrical surface should be rounded to increase the strength of the transverse edge.<\/p>\n\n\n\n

2. Arka a\u00e7\u0131y\u0131 uygun \u015fekilde art\u0131r\u0131n<\/p>\n\n\n\n

Paslanmaz \u00e7eli\u011fin elastik mod\u00fcl\u00fc k\u00fc\u00e7\u00fck oldu\u011fundan, kesme tabakas\u0131n\u0131n alt\u0131ndaki metal elastik geri kazan\u0131m\u0131 b\u00fcy\u00fckt\u00fcr ve delme i\u015fleminde i\u015f sertle\u015fmesi ciddi oldu\u011fundan, \u00e7ok k\u00fc\u00e7\u00fck tala\u015f a\u00e7\u0131s\u0131 bit kanad\u0131n\u0131n a\u015f\u0131nmas\u0131n\u0131 h\u0131zland\u0131racak, kesme s\u0131cakl\u0131\u011f\u0131n\u0131 art\u0131racak ve bitin \u00f6mr\u00fcn\u00fc azalt\u0131n, bu nedenle e\u011fim a\u00e7\u0131s\u0131n\u0131 uygun \u015fekilde art\u0131rmak gerekir. Bununla birlikte, arka a\u00e7\u0131 \u00e7ok b\u00fcy\u00fckse, ucun ana kenar\u0131 incelir, ana kenar\u0131n sertli\u011fi azal\u0131r, bu nedenle arka a\u00e7\u0131 12-15 derece olmal\u0131d\u0131r.<\/p>\n\n\n\n

Kesikleri daraltmak ve tala\u015f kald\u0131rmay\u0131 kolayla\u015ft\u0131rmak i\u00e7in, ucun iki yan\u0131nda kademeli tala\u015f ay\u0131rma oluklar\u0131n\u0131n a\u00e7\u0131lmas\u0131 gerekir.<\/p>\n\n\n\n

Bitin kesme parametreleri<\/h2>\n\n\n\n

Kesme parametrelerinin se\u00e7imi, kesme s\u0131cakl\u0131\u011f\u0131n\u0131n d\u00fc\u015f\u00fcr\u00fclmesinden ba\u015flamal\u0131d\u0131r, \u00e7\u00fcnk\u00fc y\u00fcksek h\u0131zl\u0131 kesme kesme s\u0131cakl\u0131\u011f\u0131n\u0131 art\u0131racak ve y\u00fcksek kesme s\u0131cakl\u0131\u011f\u0131, matkap ucunun a\u015f\u0131nmas\u0131n\u0131 art\u0131racakt\u0131r. Bu nedenle kesme parametrelerinde kesme h\u0131z\u0131n\u0131n 12-15m\/dak olan se\u00e7ilmesi \u00f6nemlidir.<\/p>\n\n\n\n

\"\"<\/figure>\n\n\n\n

Uygun besleme h\u0131z\u0131<\/p>\n\n\n\n

Besleme h\u0131z\u0131n\u0131n ucun \u00f6mr\u00fc \u00fczerinde \u00e7ok az etkisi vard\u0131r, ancak besleme h\u0131z\u0131 \u00e7ok k\u00fc\u00e7\u00fckse, ucun sertle\u015ftirilmi\u015f tabakada kesilmesine ve a\u015f\u0131nmay\u0131 a\u011f\u0131rla\u015ft\u0131rmas\u0131na neden olur; ilerleme h\u0131z\u0131 \u00e7ok b\u00fcy\u00fckse, y\u00fczey p\u00fcr\u00fczl\u00fcl\u00fc\u011f\u00fcn\u00fc daha da k\u00f6t\u00fcle\u015ftirecektir. Yukar\u0131daki iki fakt\u00f6r g\u00f6z \u00f6n\u00fcne al\u0131nd\u0131\u011f\u0131nda, 0.32-0.50mm\/r ilerleme h\u0131z\u0131 uygundur.<\/p>\n\n\n\n

Ak\u0131\u015fkan\u0131 kesmek<\/p>\n\n\n\n

Kesme s\u0131cakl\u0131\u011f\u0131n\u0131 d\u00fc\u015f\u00fcrmek i\u00e7in so\u011futucu olarak em\u00fclsiyon kullan\u0131labilir.<\/p>\n\n\n\n

Paslanmaz \u00e7eli\u011fi delmeden \u00f6nce dikkat edilmesi gerekenler:<\/p>\n\n\n\n

Se\u00e7ilen bitin sertli\u011fi y\u00fcksek olmal\u0131, y\u00fczey kalitesi daha iyi ve bitin tepe a\u00e7\u0131s\u0131 normal bitinkinden (130-135 derece) daha b\u00fcy\u00fck olmal\u0131d\u0131r.<\/p>\n\n\n\n

\"\"<\/figure>\n\n\n\n

1. Tak\u0131m tezgah\u0131n\u0131n \u00e7al\u0131\u015fma sesine dikkat etmek ve herhangi bir anormallik durumunda, ucun delme y\u00fczeyinde kalmas\u0131na izin vermemek i\u00e7in aleti zaman\u0131nda geri \u00e7ekmek gerekir. \u00a0<\/p>\n\n\n\n

2.So\u011futma yeterli olmal\u0131d\u0131r. Kesme s\u0131v\u0131s\u0131 konsantre em\u00fclsiyondur.<\/p>\n\n\n\n

3. Besleme 0.15 mm'den fazla oldu\u011funda, so\u011fuk i\u015flem sertle\u015ftirme tabakas\u0131n\u0131 m\u00fcmk\u00fcn oldu\u011funca kesmek gerekli de\u011fildir.<\/p>\n\n\n\n

4. Kesme s\u0131cakl\u0131\u011f\u0131n\u0131 azaltmak i\u00e7in kesme h\u0131z\u0131 m\u00fcmk\u00fcn oldu\u011funca d\u00fc\u015f\u00fck olmal\u0131d\u0131r.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"

Concerning stainless steel drill issues, it is mainly solved from the following four aspects:Select the right bit The drill material is suitable Generally, W6Mo5Cr4V2Al, w2mo9cr4co8 and other materials should be used. The disadvantages of these materials are that they are expensive and difficult to purchase. When purchasing the commonly used W18Cr4V ordinary standard high speed…<\/p>","protected":false},"author":2,"featured_media":20479,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[79],"tags":[],"jetpack_featured_media_url":"https:\/\/www.meetyoucarbide.com\/wp-content\/uploads\/2021\/03\/srchttp_2F2Fimg.chinawj.com_.cn2Fpicture2Fproduct2F20122F10-072F101103488587.jpgreferhttp_2F2Fimg.chinawj.com_.jpg","jetpack_sharing_enabled":true,"_links":{"self":[{"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/posts\/20478"}],"collection":[{"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/comments?post=20478"}],"version-history":[{"count":0,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/posts\/20478\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/media\/20479"}],"wp:attachment":[{"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/media?parent=20478"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/categories?post=20478"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.meetyoucarbide.com\/tr\/wp-json\/wp\/v2\/tags?post=20478"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}